Miksi etiketti ei pysy kiinni?
A label usually fails to stay on when the adhesive is not suited to the packaging surface material, the application surface is dirty or damp, the labeling temperature is wrong, or the facestock does not conform to the shape of the package. The adhesion problem may appear right at the time of labeling, or only during storage, transport, and use.
The problem should not automatically be solved with a stronger adhesive. At Laatuetiketti, troubleshooting adhesion problems starts from the actual application surface, the material construction of the label, and the conditions of use.
The most common causes of label adhesion problems
| Problem | Possible cause | What should be checked? |
|---|---|---|
| The label does not stick immediately | Insufficient initial tack, cold or dirty surface | Adhesive, surface temperature, and surface cleanliness |
| The edges of the label lift | Facestock that is too stiff or a challenging curvature | Material flexibility and label dimensions |
| The label comes off in cold storage | The adhesive is not suited to a cold or damp environment | Application and service temperatures |
| The label bubbles or wrinkles | Application technique, air bubbles, or deformation of the package | Labeling process and material conformability |
| Only some of the labels come off | Varying application surfaces, moisture, or process conditions | Differences between packaging and production batches |
| The label comes off during use | Moisture, chemicals, abrasion, or temperature fluctuations | Actual conditions of use and the entire label construction |
The point at which the problem appears helps narrow down the possible causes. When a label comes off immediately, the application conditions should be examined first. When a label comes off later, attention also turns to the usage environment and the long-term performance of the material.
1. The adhesive is not suited to the packaging material
Different material surfaces do not behave the same way with an adhesive. An adhesive that bonds well to glass or metal does not necessarily form sufficient adhesion to certain plastic surfaces.
Polyethylene (PE) and polypropylene (PP) in particular are typically low-surface-energy plastics. This can make it harder for the adhesive to spread across the surface and make sufficient contact.
Packaging coatings, surface treatments, roughness, and plastic additives can also affect adhesion. If the packaging manufacturer or the material grade changes, the suitability of a previously working label should be verified again.
2. The application surface is dirty, damp, or greasy
The adhesive must come into direct contact with the surface of the package. Dust, grease, oil, moisture, and other contaminants can prevent sufficient adhesion from forming.
This is especially important in production processes where product may get onto the package surface during filling, or where condensation forms on the surface of a cold package.
If the label sticks well to a clean sample package but comes off in actual production, check the condition of the package surface at the exact moment of labeling.
3. The label is applied to a surface that is too cold
Cold can reduce the initial tack of a label adhesive and its ability to conform to the package surface. Many general-purpose adhesives are not suitable for application to very cold or frozen packages.
The application temperature of a label is a different matter from its later service temperature. A freezer-grade label can retain its adhesion in a freezer even if it cannot be applied directly to a frozen package.
Where possible, measure the actual surface temperature of the package at the moment of labeling. The air temperature of the production area or cold store does not necessarily match the temperature of the package.
4. The adhesive does not have time to build sufficient adhesion
The adhesion of a pressure-sensitive adhesive can continue to develop after the label has been applied. The development of adhesion is affected by the adhesive composition, the application surface, the temperature, and the application pressure.
If the product is moved to a cold, damp, or otherwise demanding environment immediately after labeling, the adhesive may not have enough time to build the adhesion that the application requires.
Check the material-specific instructions to see whether the chosen label construction requires a certain adhesion build-up time before further handling.
5. The label material is too stiff for the shape of the package
Labels applied to strongly curved surfaces and squeezable packages need sufficient flexibility. If the facestock tends to spring back to its original shape, the edges of the label may be subjected to constant lifting stress.
Such problems can occur, for example, on small bottles, narrow bottle necks, cosmetic tubes, and squeezable plastic packages.
A more flexible facestock, a change in label size, or a different adhesive solution can reduce edge lifting. The right solution depends on the geometry of the package and the intended use of the label.
6. The labeling process does not create sufficient contact
A self-adhesive label needs sufficient and even contact with the package surface. In machine labeling, the application pressure, label placement, and movement of the package all affect how adhesion forms.
If a label sticks when applied by hand but not on the production line, the problem may be related to the settings of the labeling equipment or to how the material behaves in the machine.
In that case, check the label application pressure, roll dimensions, unwind direction, and the evenness of the labeling. The sizing guidelines from Laatuetiketti help define the technical properties of roll labels.
7. Conditions of use put stress on the label construction
A label may stick well on the production line but come off later in use. In that case, the cause of the problem may be, for example, moisture, heat, frost, oils, chemicals, or repeated deformation of the package.
Damage to the facestock can also weaken the overall durability of the label. If paper loses its structure in moisture or a plastic film changes shape in heat, changing the adhesive alone does not necessarily solve the problem.
A stronger adhesive does not fix every adhesion problem
If a label comes off because of, for example, condensation, a facestock that is too stiff, or insufficient application pressure, solving the problem requires evaluating the entire label construction and the labeling process.
What does the way a label comes off tell you about the problem?
Examining the removed label and the package surface can help identify where in the label construction the problem arises.
| Observation | What might it mean? |
|---|---|
| Adhesive stays on the back of the label and the package is clean | The bond between the adhesive and the application surface may be insufficient. |
| Adhesive remains on the package surface | The problem may be related to the internal strength of the adhesive or its bond to the facestock. |
| The edges of the label lift but the center stays attached | Curvature, facestock stiffness, or the application pressure at the edges may be causing the problem. |
| The label tears or the facestock is damaged | The durability of the facestock may not match the conditions of use. |
| The problem appears only in certain production batches | Variation in the packaging material or labeling conditions may be affecting adhesion. |
These observations are starting points for troubleshooting, not definitive diagnoses. Several factors may affect an adhesion problem at the same time.
How is a label adhesion problem investigated?
Before changing the material or adhesive, it is worth documenting how the problem appears and testing the label in the actual application.
- Determine the exact material of the package and any surface treatment.
- Check the cleanliness, moisture, and temperature of the surface at the moment of labeling.
- Compare the performance of labels applied by hand and by machine.
- Record how quickly the problem appears after application.
- Determine whether the whole label comes off or only its edges.
- Check for any adhesive residue and material damage.
- Evaluate how the label performs in actual storage and usage conditions.
If adhesion needs to be evaluated quantitatively, defined test methods for initial tack and peel strength can be used. When comparing test results, take into account the test surface, the temperature, the time elapsed since application, and the measurement method used.
What information does the label printer need to solve the problem?
Where possible, it is worth providing Laatuetiketti with a sample of the current label, the product package, and an example of the adhesion problem. A photo of a label that is coming off can also help in the initial investigation of the problem.
Also describe the intended use of the label, the application conditions, the labeling method used, and the stage at which the problem appears. Based on this information, it can be assessed whether a different adhesive, a different facestock, or a change to the technical design of the label is needed.
Are your current labels not staying on?
We help identify the possible causes of label adhesion problems and assess a material solution suited to your application. Tell us about your current label, your packaging, and your production conditions.